The tank is about 4' diameter and 5' high. I have been considering a
lined tank, but due to space restrictions the tank has to be installed
in sections. It would require welding the tank, then applying or
repairing the lining, which I would like to avoid.

On Jun 23, 10:03 am, <gabriel.to...@akersolutions.com> wrote:
> I don't know the size of your tank, but you can consider a lined (PTFE,
> PP, PE) carbon steel tank
>
> Regards,
>
> Gabriel
>
> Materials Engineering Dept
> Aker Process Ltd
>
>
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
>
> [mailto:materials-welding@googlegroups.com] On Behalf Of esharp
> Sent: 23 June 2009 13:13
> To: Materials & Welding
> Subject: [MW:2513] Brine Tank Material Selection
>
> I have an old carbon steel brine tank which is severly corroded and
> needs to be replaced. The brine solution contains ~ 10% salt (NaCl) and
> 1% caustic (NaOH) at 110 deg F. The tank is used intermittently in a
> batch process: filled for a few hours then drained and left empty for 2
> days. It is open to the atmosphere.
>
> Initialy I was considering using 316 SS, but have been reading that
> pitting could be a problem with the chloride. What material should be
> used in this application?
>
> Thanks for your help.
>
> This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this email and any attachments permanently from your system.- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...