[MW:2502] Re: KSC42W

Hi

Please conduct PMI Test on the job surface to know the chemical composition of base material.
This will give you some clue for welding consumable / procedure selection.

Regards

Prem Nautiyal
Godrej,Mumbai.


On Sat, 20 Jun 2009 08:39:23 +0530 wrote
>
>I have to do some build up/repair work on KSC42W but I don't know what
>type of base material KSC42W is and the only thing I can find on the
>web describes the component it's used in, not the material
>
>http://translate.google.com/translate?hl=en&sl=ja&u=http://www.mesco-cast.co.jp/mesco/product/ship/ship.htm&ei=4-w6Srf8EYvW6gOblqGvDg&sa=X&oi=translate&resnum=1&ct=result&prev=/search%3Fq%3DKSC42W%26hl%3Den%26safe%3Doff%26rlz%3D1T4GGLJ_enSG318SG318
>
>Has anyone worked with this material before?
>
>>
>

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...

Pages

Contributors

Blog Archive