[MW:2322] Re: Pre-WPS qualification and testing welders

Dear all,

We have steel structure procedure EN288-3 the welder qualification with EN287-1.

PreWPS procedure done without backgauging but they want to do with backgouging.

any idea..

Best Regards,


Ayhan GEDUK
Turkey Mobile:+90 5358811933

--- On Tue, 2/6/09, Ayhan GEDUK <aygedik@yahoo.com> wrote:

From: Ayhan GEDUK <aygedik@yahoo.com>
Subject: [MW:2310] Re: Pre-WPS qualification and testing welders
To: materials-welding@googlegroups.com
Date: Tuesday, 2 June, 2009, 4:09 PM

Dear  Bathula,

Thanks for your reply the procedure is steel.

It is not possible to do the welder qualification test with PreWPS.

Because of a lot of things can be change.

Thanks for your advice

Ayhan GEDUK

--- On Mon, 1/6/09, Raghuram Bathula <raghurambathula@gmail.com> wrote:

From: Raghuram Bathula <raghurambathula@gmail.com>
Subject: [MW:2295] Re: Pre-WPS qualification and testing welders
To: materials-welding@googlegroups.com
Date: Monday, 1 June, 2009, 9:26 AM

it has 13 parts
part 1 - steel/nickel
part 2 - Aluminium
.
.
.
.
etc.
in addition u must refer EN ISO 15607 ( for EN 288 -1)  
 
for material grouping refer CR ISO 15608
for welder EN ISO 9606-1 for fusion welding of steels
 
check this link for some good info http://www.gowelding.com/wp/new-standards.pdf
On Mon, Jun 1, 2009 at 10:00 AM, Ayhan GEDUK <aygedik@yahoo.com> wrote:

Dear Friends,

Our Contract based on EN288-3 for WPS qualification for WQT EN287-1

Subcontractor want to do welder qualification with pre-WPS at the same time.

Some of the place referred to updated standard that means BS EN ISO 15614-1.

conserning standard is not sufficent information.

if you have any advise please...

Best Regards,


Ayhan GEDUK
Turkey Mobile:+90 5358811933


Get your new Email address!
Grab the Email name you've always wanted before someone else does




Get your new Email address!
Grab the Email name you've always wanted before someone else does



Get your preferred Email name!
Now you can @ymail.com and @rocketmail.com
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...