[MW:2301] Re: Casting WPS/PQR

PWHT is an essential variable; you have to re-run the PQR.

--- On Tue, 2/6/09, abbey kangale <abhianu12@yahoo.com> wrote:

From: abbey kangale <abhianu12@yahoo.com>
Subject: [MW:2297] Casting WPS/PQR
To: materials-welding@googlegroups.com
Date: Tuesday, 2 June, 2009, 8:55 AM

Dear All
 
I have case for CF8M casting for Valves as per B16.34 which involves welding for internal cage fittment and ...
Foudry has done welding and then they carryout subsequent Heat Treatment 1070Deg cel.to satisfy CF8M heat treatment requirement.
 
When we asked for WPS/PQR foundry has submitted WPS/PQR for welding without PWHT and PQR is qualified without Heat Treatment requirement and for which I had taken a objection .
 
Can Group advise my objection rersolution and corrective action as casting are ready for valve asssembly for our project
 
Abhijit


Explore and discover exciting holidays and getaways with Yahoo! India Travel Click here!



Explore and discover exciting holidays and getaways with Yahoo! India Travel Click here! --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...