Dear Sabir,
Please refer page No.385 of Sec II Part - A (A234).

WPBW is mandatory Marking on the fittings. So the requirements are met
as per A234.

If there is still problem please reply to this.

Rushabh C. Kapadia

On May 8, 1:27 pm, "Zameer Mohammed" <dreamthinkw...@gmail.com> wrote:
> Dear Friends,
>
> As per our specification,
>
> 36'' EQ TEE & 36'' x 24'' RED TEE is C.S. A234 GR WPB BW.
>
> The vendor is offering - C.S. A234 *GR. WPBW*, BW
>
> How can I convince my client that *WPBW *will confirm to the Chemical
> Requirement, Tensile Requirement, for WPB.
>
> Thank you,
>
> Regards,
>
> Sabir

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...