Depends on UT technique you use but normally UT can not give reliable results on thicknesses less than 8 mm.
Normally, Maximum thickness is not a big deal since we are speaking "Pipes" here, UT can always cover all pipe thicknesses.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Normally, Maximum thickness is not a big deal since we are speaking "Pipes" here, UT can always cover all pipe thicknesses.
Ramin Kondori
QC/Welding Engineer
IWE AT 0070
On Sat, Jul 16, 2011 at 5:05 PM, ALPESH SAKHRELIYA <alpeshsakhreliya@gmail.com> wrote:
Dear allKindly provide the details of UT TESTING MIN. AND MAXIMUM THICKNESS .ALPESH SAKHRELIYA--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments