Dear naresh,
always go for higher metal chomposition
1) E8018-b2 electrode(SMAW)
2)ER80Sb2 - filler wire(GTAW)
On Mon, Jul 11, 2011 at 2:03 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
--Dear friends,I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;Regards,S.Naresh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
THANKS & REGARDS
KALYAN VVV
WELDING ENGINEER
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments