Dear 

In this case your material MTC should achieve both group (G1&G2)  for example some times we receive material like ASTM A516 achieve both groups (grade 65&70) in this case you can write in the WPS group 1&2 to group 1&2. Otherwise you have to qualify G1 to G2.



في الجمعة، ٦ شباط ٢٠٢٦، ١٢:٢١ Cezar Varin <cezarvarin@gmail.com> كتب:
Hi,

You can input in your WPS like below

P. No.1 Gr. No. 1&2 to P. No.1 Gr. No. 1&2

and it will cover all.

Thanks!


On Fri, 6 Feb 2026 at 12:07 PM dia shukr <diashukr@gmail.com> wrote:
Dear

If you have toughness test in this case you shall quilefy group number 1 with group number 2 and as ASME IX this will qualify G1to G2. G1 to G1 and also G2 to G2. For example if you have pipe(G1) and fitting (G1) and you have flange(G2) is not accepted to qualify pipe to fitting but the correct way is to weld pipe with flange or fitting with flange for procedure qualification.

في الجمعة، ٦ شباط ٢٠٢٦، ١١:٥٣ praba karan <prabakaran776@gmail.com> كتب:
Dear Experts,

Need your clarification on the following,

When the PQR(GTAW+SAW) is qualified with (Pno-1 Group no 1) with (Pno-1 Group no 2).-With impact test.

As per Sec IX, G number will be essential variable when toughness requirement is there, So can i prepare WPS for the same p number and same group number within themselves?
Like, 1)  Pno1, Group no 1 to Group no 1
          2)  Pno1, Group no 2 to Group no 2,

or is there any other suggestions to cover all groups?

Thank you..

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/90d39d5b-a8b3-4492-953d-c766aa71432en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHQEAU5Mrx5RvstghLuSAHAtQvAfDb4dk5_qoGnxLxQ6BYpESg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADxsjO9Bx97DZMLyO6AzxJ99_AYaFJ74jpThAWmzeJTd8fQGeA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHQEAU5wvGJHtxcR-ba3AesG3BKY1TLWHNkQPgh%2BMfNRmcv6iw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...