Re: [MW:35967] WPS requalification for repair weld ASME B31.3

 ASME B31.3 refers ASME Sec.IX for WPS/PQR qualification. PWHT Soak time after Repair will be considered during original PQR qualification and when Charpy Impact tests are required, below snap shot of ASME Sec.IX applies.

Inline image
Normally in Pipe Mill, MPQ (Manufacturer Procedure Qualification) with welding & Heat Treatment will be performed including repair PWHT cycles during pipe production.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday, 29 January 2026 at 08:52:28 am IST, Babur Khan <mbabur.bwp@gmail.com> wrote:


Greetings,
Thank you for your kind response.
In pur PQR, soaking time for repairs Welding not considered. 

Muhammad Babur Khan
Sent from my iPhone

On 28 Jan 2026, at 8:48 AM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


See snap shot below from ASME B31.3. No Repair procedure is required. But PWHT has to be performed after Repair. PWHT soaking time should have been added during the original PQR Qualification or Simulated test coupon including Repair soak time shall be included during Material testing.


<1769579047580blob.jpg>


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Wednesday, 28 January 2026 at 07:48:56 am IST, Babur Khan <mbabur.bwp@gmail.com> wrote:


Greetings,
Need expert opinion for the following query:
Construction Code ASME B31.3, Qualification ASME BPV Sec. IX.
One of the WPS is qualified for Low temperature Carbon steel with impact testing and PWHT. The qualification range is 20mm to 36mm. 
PWHT is applicable (Project specification). Soaking time was 1 hr 30 minutes.
Question: Is this WPS qualified for a repair weld with this soaking time? 
Is a new PQR to qualify the repair joint?

Best Regards,

<image001.jpg>

Muhammad Babur Khan Lashari
Project Quality Supervisor.
API 570, API 510, CSWIP 3.2.2. ISO 9001:2015

Mob: +966 58 2774568 / +966 51 0559680

Please consider the environment before printing this e-mail

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAN53wK16%2Bvf43xPRxmXync%3DGa42jqR7kk70ou7vyCdT9MShcZQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/411193529.3005035.1769579048563%40mail.yahoo.com.
<1769579047580blob.jpg>
<image001.jpg>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit
https://groups.google.com/d/msgid/materials-welding/A64E36D9-8FBF-467E-A12E-91D2F0370643%40gmail.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .