Re: [MW:35994] Group number selection when toughness requirement is there

Hi,

You can input in your WPS like below

P. No.1 Gr. No. 1&2 to P. No.1 Gr. No. 1&2

and it will cover all.

Thanks!


On Fri, 6 Feb 2026 at 12:07 PM dia shukr <diashukr@gmail.com> wrote:
Dear

If you have toughness test in this case you shall quilefy group number 1 with group number 2 and as ASME IX this will qualify G1to G2. G1 to G1 and also G2 to G2. For example if you have pipe(G1) and fitting (G1) and you have flange(G2) is not accepted to qualify pipe to fitting but the correct way is to weld pipe with flange or fitting with flange for procedure qualification.

في الجمعة، ٦ شباط ٢٠٢٦، ١١:٥٣ praba karan <prabakaran776@gmail.com> كتب:
Dear Experts,

Need your clarification on the following,

When the PQR(GTAW+SAW) is qualified with (Pno-1 Group no 1) with (Pno-1 Group no 2).-With impact test.

As per Sec IX, G number will be essential variable when toughness requirement is there, So can i prepare WPS for the same p number and same group number within themselves?
Like, 1)  Pno1, Group no 1 to Group no 1
          2)  Pno1, Group no 2 to Group no 2,

or is there any other suggestions to cover all groups?

Thank you..

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/90d39d5b-a8b3-4492-953d-c766aa71432en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHQEAU5Mrx5RvstghLuSAHAtQvAfDb4dk5_qoGnxLxQ6BYpESg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADxsjO9Bx97DZMLyO6AzxJ99_AYaFJ74jpThAWmzeJTd8fQGeA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .