Skip to main content

Re: [MW:35913] Clarification on usage of WPS for Particular Joint Type


Dear, Mr, Reddy,

Pl make WPS for 25 mm thk. which may cover always in all.
Regards.
R.C.DUTTA
JINDAL .


On Mon, Dec 15, 2025 at 1:21 PM kavin murugam <kavin.murugam@gmail.com> wrote:
Dear DV Reddy,
T = base metal thickness
t = weld metal thickness

Did you WPS covers both thicknesses ?

Thank you & Stay Safe!

 

KAVIN MURUGAM

+60126159644



On Mon, Dec 15, 2025 at 3:44 PM venkateswara reddy Desireddy <dvreddy82@gmail.com> wrote:
Dear friend,

Nozzle thickness 20.4mm, so your WPS thicknes must be cover 20.4mm. 20mm thick WPS not suitable to use, because 0.4 mm less thick .

Heat treatment is essential variable for WPS. If you use with heat treatment WPS, you have to do heart treatment to job also.


Regards 
D.V.Reddy.


On Mon, 15 Dec 2025, 9:14 am Shivasankar A, <shivasankar2593@gmail.com> wrote:
Hi Friends,

Refer the attached image,

In this, The cover flange thickness is 69.8 mm & The Nozzle thickness is 20.4 mm. 

the Nozzle is Set on on the Cover Flange with Full penetration Weld the groove is given on the Nozzle pipe.

The Final Fillet weld Size is 15 mm.

So may i use the WPS which Covers the thickness range from 1.5 to 20 mm?

If not, Kindly explain why?

Also Tell me the WPS Qualified with Heat treatment can be weld for the Job without Heat Treatment?

Looking for your valuable Replies. Kindly Support.

regards,
A.Shivasankar


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/6032dcdf-efef-437b-b47a-9b89a3fa83e6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKn5u98L6GEwm66itbf-z7Fz336jB%2BzzPBStijTcDaG%3DHg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAMFfK7CvihxLUKM0qVEuA-%2BWJgM1a2zwb6rOiCuP9kZ0cEmmzw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEaqp9HApjwbPsT0rWgeZnSf2Yzob9Kv3d%3DBHR%3D_KVmtyYRA2g%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...