Skip to main content

Re: [MW:35906] ASME VIII Div-1 Designed Vessel, Non U Stamped but Required CE Marking as per PED

  For PED CE‑marked vessels, ASME IX alone is not sufficient. Welding procedures must be qualified to EN ISO 15614‑1 (PED requirement), even if the vessel design follows ASME VIII Div‑1. ASME IX procedures may be reused only if supplementary testing proves equivalence and the Notified Body approves  

On Wed, 10 Dec 2025 at 17:51, Anandhapadmanabha pillaim <anandhapadmanabhapillaim1997@gmail.com> wrote:
For ASME VIII Div. 1 designed but non-stamped vessels that fall under PED 2014/68/EU, welding procedures do not need to be qualified to ASME Section IX.

According to PED requirements, the Procedure Qualification Record (PQR) must be qualified according to ISO 15614-1, and the qualification must be approved by a Notified Body.

The Welding Procedure Specification (WPS) can be based on the design code (e.g., ASME VIII Div.1), but the PQR qualification must follow ISO 15614-1 for CE marking.

In summary: For PED compliance, use ISO-qualified procedures approved by a Notified Body; ASME IX is optional if the vessel is not ASME-stamped.

On Wed, 10 Dec 2025, 4:59 pm Surendar Gunasekaran, <surendarrgs@gmail.com> wrote:
Dear Experts,

May a manufacturer use welding procedures not qualified to ASME IX for ASME VIII Div-1 designed but non-stamped vessels also required PED 2014/68/EU CE Marking ?

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/52052b03-b94c-42f9-8156-afe18417d088n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ90KGTw-t%3Dv%3DzRZRD1A_cWM0ucOCFDcYQ%3DpySe3sY%2B0O_TieA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALABf25SNTxU0SRTc0ovdmkE18yD4_06zQs96Mie6_FENtbDOA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...