Re: [MW:35779] Request for Guidance on PQR Update

Dear Sir,

 I have one doubt 

For the WPS submission

I have to Attach the new Supplementary PQR and old PQR together with the new WPS. 

In supplementary PQR format we can just add new hardness testing values rest other testing values are already in old PQR or we need to write in new supplementary PQR format also.

And we can attach old welding parameters sheet along with new supplementary PQR and in PQR format instead of PWPS no we can write Old PQR no which we are referring to.


Best Regards

Pankaj Choudhary 




On Thu, 28 Aug 2025 at 1:45 PM, sridhar cn <sridharcn305@gmail.com> wrote:

You can make a new, "Supplementary PQR" as it is safer and cleaner from a compliance and transparency 

standpoint. You prepare a new PQR document with all the welding parameters repeated from the original PQR,

plus the new hardness test results.

            

You can add a note referencing the original PQR number (i.e., "This PQR was performed under the same welding

conditions as PQR-001 (provide actual details) to incorporate the hardness testing per client requirements").


C Sridhar.


On Thu, 28 Aug 2025 at 12:21, pankaj pachahara <pankajpachahara@gmail.com> wrote:
Dear Experts,

We have a qualified PQR (P1 to P8) that doesn't include hardness testing. We're submitting this PQR for a new project, but the client requires hardness testing. To address this, we plan to:

1. Create a new PQR following the same parameters as the original PQR.
2. Conduct hardness testing and add the results to the new PQR.

We're unsure about the best approach to incorporate the hardness test results into our existing PQR documentation. We have two options:

Option 1- Add the hardness values to the original PQR as Addendum-1.
Option 2- Create a new PQR that includes all the previous data and name it as a Supplementary PQR.

Could you please guide us on the best approach to take?

Best regards
Pankaj Choudhary

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJF_nWPufvGG-sFFjNLMxN8QYd3Dqo4DHA%2B8r_ocT1_7A2SbFA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihXZ-B9EjLHi%3D%3DXq5JkE2EDs4Q5s2GLLV444PRLvC-s5Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJF_nWNZ3Qv19s6EuUM6sqPQgUd_41kUUaUdC4_B7FMMsV-jYQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...