dear sir 
 Actual project thickness :9mm ( impact required)PED
we have 14 mm thick plate SA516 G70 .if considered impact requirement as per ASME SEC IX ( WPS QUALIFICATION )we need minimum base mental thickness  9mm .we plan to weld 14mm plate decrease the thickness to 8mm .still my WPS qualified with impact 8mm To 16 mm.
My consideration is machined plate acceptable or not  which standard I need to refer 


ELAVARASAN


On Sat, 29 Mar 2025 at 10:37 AM Venkatesh Mech <venki2204@gmail.com> wrote:
Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BY70uaXej5FCPuzr%2BaUD0B0jSPObOYV0E4mkCMj17SDEr0TGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4y%3D6PGiU6r9LayDvHs%2Bvjin0MpVmWanH_URFvHxBd%2Bd-zQ%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...