Skip to main content

Re: [MW:35474] ASME B31.3 minimum distance between two erlds

Folks,

This is always a very interesting topic, I have yet to see a clear answer.

Regards,
AlanHickey.

On Tue, 4 Mar 2025 at 17:07, Naina CPECC <nmeerane@gmail.com> wrote:
it should be 4t or 100mm whichever is greater valve  is  standard practice .Some international and client standard also define this parameter. This should be mentioned in your client specification , will vary depends on clients and service  

On Tuesday, March 4, 2025 at 4:51:51 PM UTC+3 Raviraj Gohil wrote:

Client specification Min. 50 mm Distance have to be maintained


On Tue, 4 Mar 2025, 18:59 Raviraj Gohil, <raviraj....@gmail.com> wrote:

With regards to Long seam you will get from ASME Sec VIII UW-9, But silent for Circ Seam However, Good Engineering Practices and One of client specification


On Thu, 27 Feb 2025, 14:54 Noman Ahmed, <nomi...@gmail.com> wrote:
Dear expert,
can somebody provide the latest CSWIP3.1 questions and answers with a new pattern.

Regards
NOMAN

On Wed, Feb 26, 2025 at 3:55 PM Matteo Meloni <matteom...@gmail.com> wrote:
Dear Experts

I'm involved on an activity of piping welding installation, and I didn't find on B31.3 any requirement of minimum distance between 2 welds.

do you have any info? also according ISO or other standard based on your experience

thanks for your support

Matteo 
IWI-C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/d2233b5d-d28c-4e53-9e12-cbfecfc0b11fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAM%2ByfweOirWgGkCu322YeeSmv8SVb_dbp5jsTJaEt7LR4p7Dtg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/419a169f-f63b-4015-8f8a-004c86e35671n%40googlegroups.com.

CONFIDENTIALITY NOTICE: This communication, and the information it contains, is (a) intended for the person(s) and/or organisation(s) to whom it is addressed and is for no other person(s) or organisation(s) and (b) may be confidential, legally privileged and protected by law, including law of copyright. Unauthorised use, copying, forwarding or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by telephone to our head office number. We process personal data for the purposes explained in our privacy notice, which can be found here: https://www.dornan.ie/privacy-policy/ . This notice also contains information about your rights.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGFjgNH1xcokLxoXXc2kA9ngfL0wwEVEPJE8UVSj8SUboKrQyw%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...