Re: [MW:35019] thickness of WELDOLETS

Please check if the attached is useful in calculating the weld thickness.

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Monday, 20 May, 2024 at 05:25:43 pm IST, vvp....@gmail.com <vvp.varun@gmail.com> wrote:


Hi,

I have  a WPS for 6Mo with BM range 12.04 mm wall thickness max. Now i have a situation to weld a 2" weldolet on a 6" run pipe. Now weldolet groove thickness is measured to be 13.9 mm on the hub side. However the theoretical thickness is 11.905 mm. Can I weld this using the same WPS??
On Wednesday 9 February, 2011 at 8:51:31 pm UTC+4 manish kulkarni wrote:
Dear
 
The major problem with weldolets ia in procurement stage. The weld groove details, thk. are governed based on pressure rating of system.Many times high thk. weldolets are ordered even if not required as per design.MSS SP documents gives guidelines for weldolet dimensions and most of weldolet manufacturers pprepares weldlets with those details.
 
Correct way is to check required weld thk. at neck for proper weld thk. required.
 
Regards,
 
Manish Kulkarni 

--- On Wed, 9/2/11, manpreet <manpre...@rediffmail.com> wrote:

From: manpreet <manpre...@rediffmail.com>
Subject: Re: [MW:9790] thickness of WELDOLETS
To: "material...@googlegroups.com" <material...@googlegroups.com>
Date: Wednesday, 9 February, 2011, 11:07 AM

Dear Ali,

I really couldn't understand what you are asking for, but would like to detail some of the information about weldolet connection.

Weldolet might be rquired for connecting main pipe to branch (let's say dissimilar OD/thickness), now qustion arises whether weld bevel shall be completely filled out, though B31.3 calculation might not require full volume of weld, good practice is to completely fillup the weld bevel to weld line on the O-lets. Smooth transition between the pipe and the O-lets is required. Notches below the weld line shall be avoided.

Please descibe your query with quantitative information.

Regards
Manpreet Singh



On Tue, 08 Feb 2011 21:39:06 , Ali Asghari <asgha...@rocketmail.com> wrote
Dear All
According to ASME B31.3 fig328.5.4.D( SKETCH1) the thickness of weld deposit is calculated acc to 331.1.3.
Now in weldolet fittings that have unequal thicknesses in both of ends. Tb is equal to thicker or thinner thickness?why?
we need to know for calculating of governing thickness for PWHT.
regards.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4301f7b2-7da4-48a4-b78e-7c7ddfad7eb2n%40googlegroups.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...