Skip to main content

Re: [MW:35033] welder qualification

Dear Saleem,

As per the AWS D1.1/D1.1M:2020 Structural Welding Code – Steel, the qualification range for a welder who qualifies on a 6" diameter pipe with a wall thickness of 10.97 mm using the specified electrodes (E6010 for root and hot pass, and E7018 for the fill and cap passes) would be as follows:

Diameter Qualification Range

  • When a welder qualifies on a pipe with a diameter of 6 inches, they are qualified to weld pipe diameters ranging from 2-7/8 inches (73 mm) and larger.

Thickness Qualification Range

  • If the test coupon has a thickness of 10.97 mm (approximately 7/16 inches), the welder would be qualified to weld material thicknesses ranging from 3/16 inches (5 mm) to 2 times the thickness of the test coupon. This results in a qualification range of 3/16 inches to 21.94 mm (approximately 7/8 inches).

Summary

  • Diameter Range: 2-7/8 inches (73 mm) and larger.
  • Thickness Range: 3/16 inches (5 mm) to 7/8 inches (21.94 mm).

These ranges are determined based on the requirements set forth in AWS D1.1, which provides the necessary guidelines to ensure welders are properly qualified for a range of diameters and thicknesses beyond their test coupon. It is important to note that these qualification ranges are contingent on the specific procedure and test details as outlined in the AWS D1.1 code. Always refer to the latest edition of the code for the most accurate and detailed information.


On Wed, 29 May 2024 at 10:14, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

i am going to qualifying welder on pipe as per AWS D1.1

My question is if i qualify on 6" X 10.97, electrode e 6010 root+hot & e 7018 rest . whats is the qualification range for dia and thickness 



Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmtsQGJggFHLALaMyUJL%3DGzX2a3_zysrqKOz4n%2BvuFRs5A%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1pDE_Oxoi1ksNH5BV1G2MnxuBGQUv73quYx5A0y5NCyrA%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...