Skip to main content

Re: [MW:34978] Welder qualification

If F no changed we have to qualify welder for that one.
F6 qualified welder get all F6. 

On Wed, 8 May 2024, 10:39 pm saleem manhappulath, <saleemm9526@gmail.com> wrote:
Dear sir

   Please see the attached file ,
QW-423 , 


Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


On Wed, 8 May 2024 at 9:49 AM, Amol Betkar <amolbetkar90@gmail.com> wrote:

Dear Saleem,

When qualifying a welder, it's crucial to ensure that the welding procedure specification (WPS) matches the materials being welded. While it's possible to use carbon steel (CS) material for welder qualification, it's not advisable if you intend to weld stainless steel (SS) later on.

The reason is that CS and SS have different metallurgical properties, including composition, thermal conductivity, and susceptibility to corrosion. Welding procedures and parameters that work well for CS may not be suitable for SS, and vice versa. Therefore, using CS material for welder qualification with an SS WPS may not accurately reflect the welder's ability to work with SS.

For a valid qualification, it's best to use the same material (SS) for both the WPS and the qualification test. This ensures that the welder's skills are properly assessed for the specific material they will be working with in practice. If you need to qualify welders for both CS and SS welding, you should have separate WPSs and qualification tests for each material.

Regards,

AB


On Tue, 7 May 2024 at 22:06, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All


    I have a ss wps P-8 to P8, i have plan to qualify welder. Can I use cs material for welder qualification with ss wps

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmvOBHxLj-_j4XRJQ-WwN6--u79GGcQr_zND%3DQE4ye%2B6QA%40mail.gmail.com.



--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1oXRLy9Fne6Zfvw%3D0_6dRokZPdQ-7fnQanR0KPsw_TqHg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3OmtE6%2BVdX88x7ivqyUkLEYaZe%2B-mHEgJCnsXTg4PxCUYew%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEabyKnro74gum7YF49uA-Le1HXDi-GWQNonnH7j5U%2BcfKkfoA%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...