Hi Mr. James,

Thanks for the response.

In my case the heat No. is the same but having number of mother plates and subsequently daughter plates.

With regards,
Pravin

On Mon, Sep 4, 2023 at 9:29 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Inline image


According to my Interpretation,

1. Mother Coil is the initial Billet/Slab obtained from one Heat of the Furnace.
2. If  2 Heat Niumber (or 2 different rejeated slabs confirmed with Pipe Mill)  exists the word should may be considered as shall else same Heat shall be used for testing.

Thanks & Regards

J.Gerald Jayakumar



On Monday, 4 September, 2023 at 08:41:14 am IST, Pravin Mohite <praveenss224@gmail.com> wrote:


Hi Experts,

Need your advise on the interpretation of statement referred in Cl - 10.2.12.2 (b) of API 5L 46th edition for tensile retest of Gr. X65M SAWL line pipe. 

The statement of this clause which I am looking for your advise is - 'the retest specimen should be taken from two different mother coils or plate, as applicable' 

Below are the queries on this statement :
1. For the word 'should' referred in this statement. Since as per API 5L terms, 'should' refers to recommended practice & does not make it mandatory to manufacturer to comply. 

2. The term referred as 'mother Coils or plate'. Since specification doesn't referring  the term as 'Mother Coils or Mother Plate' , I can consider the other daughter plates from mother plates to take retest samples. 

My interpretation on the statement is - 
'It is not mandatory for the manufacturer to take the retest sample from the two different mother plates. He can take retest samples from the other daughter plates of same mother plates from which initial  tensile test specimen was taken '.

Requesting experts to advise on the interpretation of above statement and opinion about my interpretation.

With regards,
Pravin Mohite
+91 9664 232573




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/efe3d39d-6dcf-4b6b-8d6c-dac9c6ab4067n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/582973989.2413010.1693805127945%40mail.yahoo.com.


--
With Regards,
Pravin Mohite.
Cell - 9664232573.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADC2jB1z0xV3TurXhVjh2wDH6J42MiGuQrt8gGMp%3DO9UmEyT0w%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...