Skip to main content

[MW:34536] Alloy steel -Tube and Cladded tube sheet


Need guidance for PWHT - 

Code of Construction - ASME SEC VIII DIV 1 
Job - Heat exchanger 
Material - Tube -SA 213 T11 - 19.05 OD X 2.11 THK 
Tube sheet - SA 336 F11 CL2 , Cladded with Alloy 600 

Tube -Tube sheet joint configuration -  Groove and Fillet - 2mm -45Deg Vee with 2 mm fillet 

Welding Process proposed - GTAW  
Welding  filler metal  proposed- ERNiC3 
Query -
We reviewed the PWHT exemption in Table UCS-56-3  for P-No. 4 materials and UW-40 (f)(g) for Nominal thickness consideration and PWHT requirement 
Here nominal thickness is  Tube thickness (2.11mm )  as per UW-40 (f)(g)

Pl  advice for PWHT exemption for  above configuration of Tube to tube sheet PWHT  wrt Table UCS-56-3  or any other ref in ASME SEC VIII DIV 1 

Thanks 
Vishwas - IWE 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b7222382-b1ab-4e82-9c00-ad031880022en%40googlegroups.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...