Butter Super Duplex side with ERNi-1\ENi-1 and complete the Joint using ENiCu-7.

Thanks & Regards

J.Gerald Jayakumar




On Friday, 18 August, 2023 at 03:30:01 pm IST, Midhun murali <muralimidhun15@gmail.com> wrote:


Dear Experts,

Can anyone tell me which Electrode and Filler wire should be used for Weld Between Super Duplex to Copper Nickles.

BR,
Midhun

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/342c4e45-796c-43b9-ab8e-8131f2408cb8n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...