[MW:34456] Impact Test Temperature variation needs requalification

Dear All,

I have a WPS for P1 to P1 material, with impact test done at -30 C, another project with different material but lies within P1 and  requirement is for -60 C. Can i show the same WPS/PQR or should i do requalification.