Thursday, August 3, 2023

[MW:34460] Re: HIC Test + NACE

Fluid service or exposure to an oilfield environment containing Hydrogen Sulfide (H2S) can cause cracking of materials by damage mechanisms such as SSC / HIC / HSC / SCC /\ SOHIC / SWC / SZC.

On Monday, 24 July 2023 at 18:10:11 UTC+3 Vignesh Pal wrote:
When do we specify HIC requirements along with NACE Sour service requirements?

In many case NACE + HIC are mentioned...what does this mean?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80f37fa7-3a5d-4cef-8b1e-be4ada8ad5f4n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...