Friday, August 18, 2023

[MW:34503] Re: Super Duplex (32205) To Copper Nickle 90/10 (SMAW + GTAW)

Pl. furnish below inf
1)What is type of joint 
2)What is service 
3)Operating temperature 


On Friday, August 18, 2023 at 3:30:10 PM UTC+5:30 Midhun murali wrote:
Dear Experts,

Can anyone tell me which Electrode and Filler wire should be used for Weld Between Super Duplex to Copper Nickles.

BR,
Midhun

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f3c8249e-d9a2-4d78-a51f-351440222749n%40googlegroups.com.