[MW:34507] ALUMINIUM 6082 -T6

Dear Experts 

ALUMINIUM 6082 -T6 - 32mm , 20 mm , 16 mm plates 
32mm ,-32mm- Butt joint
 20 mm-20 mm-Butt joint
16 mm - 16 mm -Butt joint
Above plates are jointed through butt joints  .
Welding Process - GMAW 
Gas - Argon 
Filler wire  - ER4043

Due to job part length , there is distortion at the vicinity of butt welds. So Cold straightening operation was carried out on Press. The weld/HAZ cracking is observed  immediately the press load is commenced

Pl. suggest suitable action for Welding/cold straightening 

Thanks 

Vishwas - IWE





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/597ef31f-53c7-4c81-9924-cbbdd688c49an%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...