Dear Prashant ,
Your  query  starts with PQR but it is ref to WPQ range. 

As I  understand correctly , you are referring  to Qualification range of WPQ  .So sending related  ASME SEC IX  Table for your ref.
 .Accor , production welds can be welded 

Thanks

Vishwas- IWE
position QW461.JPG


On Wednesday, August 9, 2023 at 9:04:29 AM UTC+5:30 GALAXY INDUSTRIES PRASHANT PANCHAL wrote:
Dear Experts,

Kindly clear my confusion for PQR qualification

The welder is qualified for 10mmthk Goove weld in plate. Is he eligible for welding dia 42mm sch 40 pipe for welding fillet joint. 

Kindly acknowledge the same. 


With Best Regards, 


Prashant Panchal 


M/s. Jove Engineers Pvt Ltd,
R-386, TTC Industrial Estate,

Rabale, Navi – Mumbai-400701.

Mob: +91-98200-82842 
Email : 
pipa...@live.com
            
galaxy....@gmail.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c3dd941-7b9f-4dee-ae9d-34b08f873e24n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...