Re: [MW:34488] Welding materials SA-240 310s (P.no8) to SA-213 T11 (P.no4)

Pl refer API RP 582 



On Monday, August 14, 2023, 3:26 PM, Mohamed Elsayed <m.sayed0994@gmail.com> wrote:

Hello dears
I'm going to weld SA-240 310s (P.no8) to SA-213 T11 (P.no4), but I don't know what is the proper electrod or filler metal to weld this material, so help me please

--