Dear Prashant,

As per QW 461.9 table, Plate-Groove weld qualification, the welder can weld 42mm pipe fillet weld.  For position of Fillet weld refer your WPQ and Table QW 461.9.

Ensure WPS and PQR available for particular material grade. 

Thanks and regards 
Rathinavel 

On Wed, Aug 9, 2023, 9:04 AM GALAXY INDUSTRIES PRASHANT PANCHAL <pipanchal@live.com> wrote:
Dear Experts,

Kindly clear my confusion for PQR qualification

The welder is qualified for 10mmthk Goove weld in plate. Is he eligible for welding dia 42mm sch 40 pipe for welding fillet joint. 

Kindly acknowledge the same. 


With Best Regards, 


Prashant Panchal 


M/s. Jove Engineers Pvt Ltd,
R-386, TTC Industrial Estate,

Rabale, Navi – Mumbai-400701.

Mob: +91-98200-82842 
Email : 
pipanchal@live.com
            
galaxy.panchal@gmail.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DS0PR12MB777126D6C9ED6ECC3BE7765DC30EA%40DS0PR12MB7771.namprd12.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPHaPBKs16Q3j%2By0%2BzBDHKDjk%3DioRrB5WvormN_WH5W0vfigMA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...