Re: [MW:34477] Re: Argon Gas Generator

Hi All,

Case details: 

Tube sheet base material is SA-266 2/4N
Explosion bonded Cladded face (10mm) with - CrNi 90/10.
Tube material =  SB-111UNS C70600 (CuNi 9010), FINS-ALUMINIUM

Question: What will be the weld material for strength welding in between cladded face material (CrNi 90/10) to  SB-111UNS C70600 (CuNi 9010).

Vendor proposed silver brazing, need help to evaluate it and to avoid any expected repair after operation of HEX. What should be the weld filler material?












On Wed, Aug 9, 2023 at 6:34 AM Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Hello All,

As you might be already aware, the price & demand for the Argon is increasing rapidly and we have to find a suitable option as a replacement especially for Gas Arc Welding.

So one of the options I am looking at present is to replace the cylinders with an Argon Generator.

If anyone has any inputs for setting up Argon Generator at site & the pros and cons of it please share.

If anyone has the same experience on setting up the same, please provide the details of the suitable supplier.

Regards,

Best regards,

Gowtham Rajendran

Welding Engineer 


On Sat, 5 Aug 2023 at 10:13, Gowtham Rajendran <rajgowthamiwe@gmail.com> wrote:
Hello All,

As you might be already aware, the price & demand for the Argon is increasing rapidly and we have to find a suitable option as a replacement especially for Gas Arc Welding.

So one of the options I am looking at present is to replace the MAG welding process with Argon Generator.

If anyone has any inputs for setting up Argon Generator at site & the pros and cons of it please share.

If anyone has the same experience on setting up the same, please provide the details of the suitable supplier.

Regards,

Best regards,

Gowtham Rajendran

Welding Engineer 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABLAf1J1xL0WKGgtajBQei9SVmv%2B21Y3_qG32va7qrD8aURD%2BQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADVhYFjy62Et1cdyJMKKchjWsLSs82fu8mjDeso6LBNiZ-Hcuw%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...