Wednesday, August 16, 2023

[MW:34491] Re: ER70S-2 and ER70S-6 (GTAW Process)


You can write ER70S-6 with a note in WPS that :

Mn content shall not exceed 1.6 % 
Si content shall not exceed 1.0 % 

Thanks
VIshwas - IWE 




On Monday, June 3, 2019 at 7:48:39 PM UTC+5:30 K K wrote:
Dear All,

My PQR is qualified with ER70S-2.

Can I use ( Mention) ER70S-6 in WPS.

Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/44b55841-6c7a-4e35-8a10-4879eca1ff20n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...