[MW:34473] Re: Filler Selection for welding IS 1239 Pipe

Pl. send MTC of  IS 1239 (Ungalvanized) Pipe. 

On Wednesday, August 9, 2023 at 9:04:29 AM UTC+5:30 GALAXY INDUSTRIES PRASHANT PANCHAL wrote:
Dear Experts,

Can we use ER110S-1 for welding IS 1239 (Ungalvanized) Pipe. 

Kindly acknowledge the same. 


With Best Regards, 


Prashant Panchal 


M/s. Jove Engineers Pvt Ltd,
R-386, TTC Industrial Estate,

Rabale, Navi – Mumbai-400701.

Mob: +91-98200-82842 
Email : 
pipa...@live.com
            
galaxy....@gmail.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/76ce0b97-34b3-4414-a7af-8f41585ba9ban%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...