Re: [MW:34494] Re: ER70S-2 and ER70S-6 (GTAW Process)

Any advantage in writing chemistry in WPS, how it will help welders. 

On Wed, Aug 16, 2023, 2:22 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:

You can write ER70S-6 with a note in WPS that :

Mn content shall not exceed 1.6 % 
Si content shall not exceed 1.0 % 

Thanks
VIshwas - IWE 




On Monday, June 3, 2019 at 7:48:39 PM UTC+5:30 K K wrote:
Dear All,

My PQR is qualified with ER70S-2.

Can I use ( Mention) ER70S-6 in WPS.

Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/44b55841-6c7a-4e35-8a10-4879eca1ff20n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMhmVQEGN0sLKfNYdbyN3%2B3vBkd%3DdASGymU3-6068f6Vw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...