Re: [MW:33411] MPI for duplex stainless steel

DSS is not good magnetize because it's structure Consists of two dual phase;  paramagnetic phase  called austinite 50% and magnetize phase called ferrite 50% , so you will find moderate magnetization not be well in inspection, it's better if you use PT method instead of MPI.

On Tue, Aug 30, 2022, 7:51 AM Moossa Kutty <moossakuttypk@gmail.com> wrote:
Magnite not catch properly on the DSS materials , so result is wrong, as per MPI procedures not allowing also 

On Mon, Aug 29, 2022 at 5:52 PM Mohd Siraj <mohd52100@gmail.com> wrote:
hi gents,

can we do Magnetic particle test for duplex stainless steel

i believe we can do since DSS is ferromagnetic material

whats expert opinion?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb9b8ceb-4164-459d-ac06-9d51033706dan%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKgLv__ygYTZsADnA4F-XFqy0G86LV7cZxbyzO-Q2dMi4D1Vww%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK-7o_PnE%3D0rg68EpuG1nsh8sBYwSVmQwNd5YtOSWVv1fcHwKg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...