My opinion with experience Copper to SS welding is not compatible
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1295258517.2205182.1661433554582%40mail.yahoo.com.
You can braze or vaccine braze with BAg8 or similar filler
Hegde
-- On Thu, 25 Aug 2022 at 18:04, 'J Prinsen' via Materials & Welding<materials-welding@googlegroups.com> wrote:--You can try with inconel 625 or Nickel 200, or buttering the stainless steel with either 625 or 200 and then weld with the same consumable to the copperI' ve seen welding with a copper consumable in the past, but there is a high risk of hot cracksRegardsJurgen Prinsen IWEVan: "Mohd Siraj" <mohd52100@gmail.com>
Aan: "materials-welding" <materials-welding@googlegroups.com>
Verzonden: Donderdag 11 augustus 2022 17:09:48
Onderwerp: [MW:33377] Re: Weld Copper to Stainless Steel 304pl share exact specification of material to be weld with thickeness.for any question to be answered quickly , you could provided suffiecent details so that other can understand your requirement like code interpretation querry.--On Saturday, July 30, 2022 at 5:00:55 PM UTC+3 Sohil Mehta wrote:Dear Sir,Kindly suggest consumables for welding of Copper to Stainles Steel.Thank you.Regards,Sohil Mehta
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c84d8a39-6385-4d7d-9c48-df32d4658770n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2056395243.42875647.1661429976858.JavaMail.zimbra%40online.nl.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1295258517.2205182.1661433554582%40mail.yahoo.com.
Comments