Friday, August 26, 2022

Re: [MW:33399] Boroscope Requirement

Hi,

I used the below which gives good quality video / Images in the 7 - 10X magnification.
While assessing the defect consider the magnification also.



Regards
V. Kingsly Geo.


On Thu, 28 Jul 2022 at 07:25, Sudhakar Kuppuswamy <sudhakarceng@gmail.com> wrote:
Hi,

In the market there are several model available, the best ones are from GE  and Olympus . These models are having only few meters (1 to 1.5 meter max) cable length, so it can be effectively used for piping works. 

If you are looking for pipeline works, you need go with custom made borescope/videoscope units .

Regards,
Sudhakar K 


On Mon, 25 Jul 2022 at 12:14 PM Deepan Pan <deepanji90@gmail.com> wrote:
Dear Experts,
We have a requirement for boroscope (checking the internal pipe condition and Weld root penetration ). Please suggest the best boroscope which is available in market.

Regards,
Pradeep.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/abbb591e-16e7-4580-ade0-36997b2debd2n%40googlegroups.com.
--

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhakarceng@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABF8NYVT3EUG-zo0yPVZLZJ0EO6hgGQ_cSnGrkqQVL8NeTYW2A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ-tC0GXGdDU7NCdUVoAC8b%2BztLK-QdboUKzV5TA6s03-Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...