Thursday, August 25, 2022

Re: [MW:33395] NDE REQUIREMENT FOR P11 MATERIALS AFTER PWHT

REF ASME B31.1,  136.4, No time limit but for materials like P3,4,5 etc, NDE is to be done after PWHT only unless otherwise specified

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Aug 25, 2022 at 2:02 PM V.kishore raju <vkishoreraju55@gmail.com> wrote:
Dear all
can i perform NDE inspection like RT,HT,MT,PMI before 48hrs from the pwht time for P11 materials,is there is any specific code regarding this matter.
kindly conform me.

thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cf61cc50-a0d5-4151-b940-15a1122c12cen%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNxUBMJrXY6CZsQABa5doURE6%2B%3DZedNNuVSY%2BO6BQ0pWA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...