Re: [MW:33395] NDE REQUIREMENT FOR P11 MATERIALS AFTER PWHT

As my experience after 24hrs once done PWHT can be processed to all kind of NDT


Thanks & Regards
Thermoheat 
Heat treatment 

On Thu, 25 Aug 2022, 17:13 Ajay Gupta, <ajaygupta025@gmail.com> wrote:
That will not be any problem, please ensure NDT shall be carried out after 48 Hrs of PWHT not immediately after heat treatment.

On Thu, Aug 25, 2022 at 2:02 PM V.kishore raju <vkishoreraju55@gmail.com> wrote:
Dear all
can i perform NDE inspection like RT,HT,MT,PMI before 48hrs from the pwht time for P11 materials,is there is any specific code regarding this matter.
kindly conform me.

thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cf61cc50-a0d5-4151-b940-15a1122c12cen%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMBBuP2NWOzYvMiemC%3DZBpKLh7OuBH8ssw7fOsNTvYEU01OWUQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADTt-98w22_0%3DF63Gj7abvd%3D7Ojb3C5jRznvh_RrV9aNe%2BCjCQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...