Thursday, August 18, 2022

Re: [MW:33386] Recommended Paint Specification

Dear Team 
Which electrode I have to use for disimiler E355 & 316 material
Pl suggest 309 or 309L

Thanks & Regards,

Rupam Manna
Mobile:07894459583

Sent from RediffmailNG on Android




From: "finitei...@gmail.com" <finiteinjustice@gmail.com>
Sent: Thu, 18 Aug 2022 13:02:48 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:33385] Recommended Paint Specification

I need a recommendation for suitable paint specification of internal painting (bottom plate & shell course) of petroleum refinery intermediate product tank with steam coil.

Due to temperature epoxy or polyurethane paint spec may not last.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https:roups.google.com/d/msgid/materials-welding/b1c42aaa-3826-47ec-b183-cde89642ec31n@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1660807968.S.8618.11602.f4-234-102.1660811192.30476%40webmail.rediffmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...