Wednesday, August 3, 2022

Re: [MW:33352] Reg Flange Serration Damage

Hello sir 
Without material build up at that damage place, how machining is possible??? It will reduce the dimensions I think

On Wed, Aug 3, 2022, 13:59 Sudhir Kumar <sudhir18092@gmail.com> wrote:
Flange serration in place is possible  without any welding (do not require PWHT). Need to hire contractor who is having specialised machine. 
As its not commonly used, service cost would me higher.

Regards 

On Wed, 3 Aug 2022, 12:33 srinivasa rao, <srinivaskona25@gmail.com> wrote:
Dear All,

We have found Damage on the Flange Serration A 350 LF2 CL1 standard , 300 #. 
Can we make the repair by weld buildup and Make new Serration . Also is it necessary to make any Heat Treatment after the serration ?

Pls advise.

Attached photo for reference. 

Srinivas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKqa_5vs9nM%3Dsaw6B_7%3DVvmGxRzj_h1wmr10fZkuNRqrkJnxaA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACEhC4Z41RW2bzs0yJmFw2TPsbo1YpZMADPvjccdO0sDVLBmzw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__5XBQXcyobOZOeLfQipWo7yPUc6Sz2DYy86K2UO9WY6A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...