hi, Mr denaouda,

you can refer procedure provided and the last pl contact pipe mfg for final pressure and holding.(i think who is mfg CPI,oman ?)

there is two one test is strength test of 4 hr and second is a leak test of 24 hr at design or 1.1 design.

regards,
Siraj.
On Wednesday, August 3, 2022 at 11:21:29 AM UTC+3 Benaouda Mezrar wrote:
hi expert 

could anyone have a procedure for HYDROTEST pipeline GRE 

thanks



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f4a6512d-2387-497b-9704-874cba33778an%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...