Thursday, August 4, 2022

[MW:33359] Re: Reg Flange Serration Damage

It is better to make new serration by machining, avoid any weld repair.

Regards,

Mukesh Shah
Alliance Pipes & Fittings
sales@alliancefittings.net

On Wednesday, August 3, 2022 at 3:04:02 PM UTC+5:30 srinivasa rao wrote:
Dear All,

We have found Damage on the Flange Serration A 350 LF2 CL1 standard , 300 #. 
Can we make the repair by weld buildup and Make new Serration . Also is it necessary to make any Heat Treatment after the serration ?

Pls advise.

Attached photo for reference. 

Srinivas

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fd6b7fe3-a44e-4d23-bf86-29189715723fn%40googlegroups.com.

No comments: