Tuesday, February 1, 2022

[MW:32795] Pitting corrosion acceptance criteria for steel plates

Dear,
Is there any allowances or acceptance criteria for pitting corrosion in offshore structural plate material (S355 JR)…
And also how to measure the depth of pitting size…
Kindly advise…
Thanks & Regards 
KrishnaMoorthy

--