Dear,
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a4b7dd41-2100-421f-abca-0829e2fbc6d0n%40googlegroups.com.
Is there any allowances or acceptance criteria for pitting corrosion in offshore structural plate material (S355 JR)…
And also how to measure the depth of pitting size…
Kindly advise…
Thanks & Regards
KrishnaMoorthy
-- https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a4b7dd41-2100-421f-abca-0829e2fbc6d0n%40googlegroups.com.
Comments