Yes you can. Normally for a higher temperature range and the associated cost.
Thanks & Regards
J.Gerald Jayakumar
On Thursday, 24 February, 2022, 08:14:24 am GMT+4, Manikandan J <mechmani22@gmail.com> wrote:
Dear Sir,
Thanks.Can I use ERNiCRFe-2 as per API RP582?
Reagards,
Manikandan.
On Wed, Feb 23, 2022, 8:16 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
--ERNiCrMo-3 or ERNiCrMo-10Thanks & Regards
J.Gerald Jayakumar
On Wednesday, 23 February, 2022, 08:07:20 am GMT+4, Manikandan J <mechmani22@gmail.com> wrote:Dear All,--What is the Suitable Consumable for CS to Inconel 625 Material for GTAW & SMAW Material.Process : GTAW & SMAWRegards,Manikandan
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNk3ySUGffFw_3pVtosNQj_4AS3S-w9HKS4Bud54qEbDQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/170498679.747898.1645593177177%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmPF0da%2BkKOe00yGfgMAeoNJXd03NCXK8N%2BrsQ%3DL%3D7oWsA%40mail.gmail.com.
Comments