Hi,

 

Your query does not specify the intended service? However, application of Duplex Stainless steels in pipelines are typically for offshore O&G carrying and processing pipelines. DNV guidelines are followed a lot for such design conditions. You may take a look at this attached specification and read through some of the highlighted guidelines. Usually for such pipelines involving Duplex Stainless Steels many of the technical requirements are client driven. If your project has specific requirements those would be more binding that the attached specification.

 

 

Thanks.

 

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf of Benaouda Mezrar

Sent: February 17, 2022 5:15 AM

To: Materials & Welding <materials-welding@googlegroups.com>

Subject: [MW:32887] Qualification of WPS for DSS

 

 

Hi expert

 

In which code I can find the essential variable for qualification of the WPS for DSS pipeline thanks for your help friend and have good day

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com <https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com?utm_medium=email&utm_source=footer> .

 

 

 

________________________________

 

<https://www.avg.com/internet-security>   This email has been checked for viruses by AVG antivirus software.

www.avg.com <https://www.avg.com/internet-security

 

 

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com <https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com?utm_medium=email&utm_source=footer> .

 




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...