Hi Brijesh,
For your query GTAW process only for 4.78 mm as per sec ASME SEC IX code min 1.5 to 2T for process yes we can use PQR but WPS need to do. Hopely your job not required impact test if not above details ignore
On Sat, Feb 26, 2022, 12:08 PM Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:
Dear All,--I have PQR of GTAW + SMAW process for P1G2 to P1G2 (SA516 GR.70 to SA516 GR.70)PQR Plate thickness = 10 mmGTAW welded = 4 mmSMAW welded = 6 mmWPS range qualified = 1.5 to 20 mm.Now, My query is, can i use this WPS for WPQ by GTAW process only?I want to qualify my welder on 1/2"NB X SCH 160 (4.78 THK) pipe with only GTAW process using this WPS.Kindly Clarify Experts........Regards,Brijesh Maurya
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_eMeAVHXjg29UVz9HjnkscfsZX9-0hGMc-rOZCqWsA1C_A%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYwZWkT-tGxqYHMd24-HyPg8t_Q6A3itywMti8uGTsigyg%40mail.gmail.com.
Comments