Re: [MW:32936] WPQ of single process having combination PQR

Hi,

Seperate WPS for GTAW process to be prepared and approved using the available PQR for GTAW + SMAW .

Thickness range qualified for this WPS for GTAW process will be 1.5mm to 8mm with which WPQ can be done on 4.87 mm thick pipe.


Regards,
Anup


On Friday, February 25, 2022, Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:
Dear All,
I have PQR of GTAW + SMAW process for P1G2 to P1G2 (SA516 GR.70 to SA516 GR.70)
PQR Plate thickness = 10 mm
GTAW welded = 4 mm
SMAW welded = 6 mm
WPS range qualified = 1.5 to 20 mm.

Now, My query is, can i use this WPS for WPQ by GTAW process only?
I want to qualify my welder on 1/2"NB X SCH 160 (4.78 THK) pipe with only GTAW process using this WPS.

Kindly Clarify Experts........


Regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_eMeAVHXjg29UVz9HjnkscfsZX9-0hGMc-rOZCqWsA1C_A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutbqRkgynupruYbHrg7hmCbgchETm9uXWKHHAXU%3DQsowag%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...