Re: [MW:32901] RE: 32887] Qualification of WPS for DSS

But This Pipeline are for onshore, and the service is gas
so could I use the DNV for the pipeline at onshore ?
or is there another code for qualification ?

Le ven. 18 févr. 2022 à 01:24, <pgoswami@rogers.com> a écrit :

Hi,

Your query does not specify the intended service? However, application of Duplex Stainless steels in pipelines are typically for offshore O&G carrying and processing pipelines. DNV guidelines are followed a lot for such design conditions. You may take a look at this attached specification and read through some of the highlighted guidelines. Usually for such pipelines involving Duplex Stainless Steels many of the technical requirements are client driven. If your project has specific requirements those would be more binding that the attached specification.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf of Benaouda Mezrar
Sent: February 17, 2022 5:15 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:32887] Qualification of WPS for DSS

 

Hi expert

In which code I can find the essential variable for qualification of the WPS for DSS pipeline
thanks for your help friend and have good day

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANKYR7s_MAyByoWc2Vkt0P92JxoLZ0SZ4cWJOvosnr7FCV2Wcw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...