Re: [MW:32851] API 5LC GR LC65-2205

Please check API5LC, an old edition attached.

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 10 February, 2022, 05:05:32 pm GMT+4, Benaouda Mezrar <mezrarbenaouda4@gmail.com> wrote:


HI friend 
in wich code i can find the metal API 5LC gr LC65-2205 ? (API SPECEFICATION 5L or table QW/QB-422 of ASME IX)
could any one help me please 
thanks  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/218d1f82-f407-452a-b84f-820796e594a9n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...