Re: [MW:32886] Feritic Steel

Hello SN, 

You can refer to the International- ASM handbook. Please find the attachment

On Thu, Feb 17, 2022 at 10:05 AM SN <suryawanshinileshj@gmail.com> wrote:
Dear all,

As there any supporting national or international standards available which  exactly spell the definition of feritic steel as client was a reference for the same.

Thanks

On Thu, 17 Feb 2022, 9:42 am Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
misunderstood asFerritic stainless steel.  All carbon, low alloy steel are ferritic steel which can be heat treated
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Feb 17, 2022 at 8:52 AM Jenish Mistry <jenishmistry1992@gmail.com> wrote:
Dear sir,

Why it can not hardened by heat treatment?

By which process it can hardened ??


On Wed, Feb 16, 2022 at 1:00 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Less Carbon, High Chrom and some small  addition of alloying elements Nb, Ni etc
U can not hardened by heattreatment

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 16, 2022 at 8:52 AM SN <suryawanshinileshj@gmail.com> wrote:
Dear all,

What is the exact defination of ferritic steel as per ASME or ASTM or EN standard.

Kindly clarify

Regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7M_Yv5pZ2eRgWjLGTcXPwtBRTM0S5o1idRkeMAmidU-TA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNDwXmnAYhfszjsxCU-GPvQZMk%3DtnDcTj2BGehpPK7v_w%40mail.gmail.com.


--
Thanks for your best support.

Regards,
Jenish Mistry
09033476117

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_cDKpB79gZWrMbOqCsWxznU1-47GDPmj8cC5cKpXcdXMQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOnQDjgsensGHTq9-F8YmGb8wCN2PhoZny3ZG6Kv3TLnw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7MkgTJkWBytrF8vA1Cu4ssxrs1KHMp5QMKWi1%2BMQYNDrA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-ztdEuiN6twiONEx3es_k5TCY5gVqGQTRNc%2Bitgda6qQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...